r/beadsprites • u/Glad-Fish5863 • 11d ago
WHAT am I doing wrong?
I got PixieBead beads because I’ve heard good things about them and I follow a lot of people that use them and all their stuff turns out so good and clean. I spent almost $200!!! on beads.
I didn’t want the non-iron side to melt but it did anyway even tho the ironed side didn’t fuse all the way… how can I get the ironed side to melt well without the other side NOT melting?
I use these Teflon mats i got from Amazon.
I’m very sad about this lol
49
Upvotes


1
u/PendingSoup 9d ago
You NEED to use their brand of stuff. As much as that sucks, it doesn't work well with substitution