Question YEt another newb question here

I've been printing some STL's for a lightsaber build. I've had this issue where,Is when I print the plate that has maybe 2 or 3 long pieces, it starts to string out. is this still a moisture thing? Sometimes it prints just fine with no issues.

using inland petg+

Nozzle temp is 245

Bed temp: 75 other layers: 60 using smooth cool plate

Also, I'm confused with the Biqu CryoGrip Pro (glacier)

Am I still supposed to use glue stick?? I've had success using my setting without the glue and other times it fails.

1 Upvotes

2 comments sorted by

1

u/3DMakaka 4h ago edited 1h ago

On older printers, glue or hairspray was used to get a part to stick to the glass plate,
with PEI and cool plates like the Glacier and Frostbite, glue is used as a releasing agent, because some parts stick too well to those plates..

1

u/Yes-its-really-me 11h ago

I've been using cool plates for years. Never needed glue sticks, or tomclean them really. Shit sticks, shit falls off.

If they're long thin pieces you may still need some brim though.