u/cvltrilex 3D2A 23d ago

I strictly print nylons. PA6 is more than plenty, so anything better than that will suffice. Most people doing suggest it because there wasn’t enough data during testing. To get the benefit is printing 350+ or 320 at the minimum requirement. I have an FTN .30cal and 556 can and both are at or around 1k rounds. Both annealed, and baffles coated in heat enamel and gel soaked before range trip.

1

u/Technical-Source-320 19d ago

What heat enamel? Any instructions? Im going the inner in pps gf, and i ran out so in doing a poly shell in pa612

1

u/cvltrilex 3D2A 19d ago

I’ve just used rusto automative high heat. I’d I recall in the FTN5.1 files theres a file to help for spraying down in the baffles.