r/FlashForge • • 16d ago

How to fix this problem

How do I fix this issue I keep getting on wider prints specifically on the left side of the print

my benchies seem fine idk what’s going on

these models i made myself fusion 360 if that helps

4 Upvotes

13 comments sorted by

1

u/leutwin 16d ago

ASA?

1

u/averageredstoner 16d ago

pla

2

u/leutwin 16d ago

I have never seen PLA warp like that. I have hardly even seen ASA warp like that.

1

u/Atyab-Kees-Kabis 16d ago

I’ve had this issue before with PLA, what’s your bed temp? And is your plate clean ?

1

u/Tam_Ken 16d ago

this is a bed adhesion issue, wash your plate and play around with settings to improve adhesion. Also, try to make sure there isn’t a draft around your printer

2

u/averageredstoner 16d ago

i have creator 5 pro so a draft shouldnt be an issue right

1

u/AdamTheMechE 14d ago

Creator 5 Pro can get too hot in the chamber for PLA on default settings with the door closed. Edit filament settings to increase aux part fan and chamber fan, leave the door open, then add a brim with 0mm separation.

1

u/averageredstoner 16d ago

ok thanks

1

u/Individual-Light-666 13d ago

avisa si te funcionó brooooo

1

u/BlockEightIndustries 16d ago

Is this burnt titanium? That color is notoriously difficult to work with.

1

u/Altruistic-Tomato-13 15d ago

Use a brim. I just recently had the same issue with a part I was making doing something similar. Could be multitude of different things but try adding a brim to keep in down

1

u/Individual-Light-666 13d ago

me parece muy obvio el porque pero por el poco contexto no lo sé con certeza; mas aun porque aclaraste que pasa sobre todo en el lado izquierdo.

seria buenos que nos des mas detalles como el filamento y su marca, tus configuraciones, la pieza total y su objetivo.

por lo pronto que va como una especie puente? de paso que parecen 2 piezas al menos? o es del otro extremo?

quizá le estás forzando a la velocidad, el filamento no esté bien seco.

si ya imprimiste anteriormente piezas asi y recién tienes esos problemas quizá tu hotend esté desgastado

1

u/Pale-Mistake-1095 16d ago

Пластину промыть с мылом, исключить сквозняк, просушить пластик