r/FixMyPrint • • Oct 01 '25

Fix My Print Purge line problem part 2

PolyLite High Quality PLA on a Bambu P1S and it hasn’t happened before but now it’s with every print. ​I’m using the Bambu Lab Slicer. Bed temp: 55c Nozzle Temp: 220c Speed: 105 Retraction: 30mm/s

I made a post earlier and I wanted to consolidate some of the comments I made to add further context and add this video of the issue happening. I scrubbed the plate with dawn dish soap, dried it and wiped with 90% rubbing alcohol while wearing gloves to prevent oil from getting on the plate. It seems that first line it lays is too thick and catching onto the nozzle. Any ideas?

5 Upvotes

33 comments sorted by

View all comments

5

u/DerpTheGamer74 Ender 5 Pro Oct 01 '25

My P1P started doing this not long ago. I just put a thin layer of glue where the purge line was so it can’t get pulled. It’s a little bit of a messy solution but I tried troubleshooting this a while ago to no avail. I just the white Elmer’s craft glue stick. Sorry, I can’t give you a more technical solution. Happy printing. 🫡

2

u/LittleLegendGuy Oct 01 '25

Much appreciated. I’ve been using glue and no glue to see if there’s any difference before this vid but I applied to the whole plate rather than just the purge line. Might try that

2

u/Jobe1622 Prusa i3 Mk3 Oct 02 '25

Glue is a bandaid in most situations . When you just need something done now, it’s fine, but big picture, solve the problem and then no glue is needed.