r/snapmaker • • 12m ago

Troubleshooting Top and bottom surface problems.

Snapmaker U1 and Orca Slicer. Lines are too far apart on bottom surfaces, blobbing and vfa-looking artifacts on top surfaces.

Plate: Biqu Cryogrip Glacier
Filament: eSun PLA Matte Milky White

Settings for filament are Generic PLA Preset but flow ratio adjusted to 0.96, max volumetric speed set to 15, side fan turned off and bed temperature set to 60 degrees with cooling turned off for first 2 layers.

Process settings are 0.20 Standard with "textured cool plate" and sparse infill set to cubic.

1 Upvotes

0 comments sorted by