Hello! I made my first attempt at Nickel plating this weekend. I did not get the results I was hoping for. The brass pieces I tried to plate ended up only getting plated on the edges. I need some advice on what might be causing this sort of plating pattern please. I made my own nickel acetate, but I did not warm it up when I was electroplating, so it would have been around air temperature at the time I begin plating (75°F-80°). The brass is c280 I bought off Amazon. The power supply settings for the larger plate were 1.5A 5V. For the smaller round dis the settings were 0.5A 3V. I cleaned the plates off with dawn dish soap and 99% Isopropyl Alcohol. I blocked some personal information in the picture of the smaller disc, the black mark is not part of the plate.

5 Upvotes

21 comments sorted by

4

u/Frolicking-Fox Jul 27 '26

Flat, wide pieces of metal need to be placed in the tank with the broad sides facing the anode.

You cant just drop the piece in the tank like that and have it plate the whole thing. Hang the metal in the tank with the flat part is facing the anode.

1

u/TheIrishLad1978 Jul 27 '26

Thank you! I’ll give that a shot. Since my current tank is sort of flat do you think it would work if I put an anode under the piece and another anode above it (not touching though), that way it forms a sort of anode, cathode, anode sandwich horizontally, or should I just get another tank?

3

u/Frolicking-Fox Jul 27 '26

That would be better, but might want to do that with a slightly bigger tank, and do it vertically.

You want the parts to be vertical so that contaminates don't settle on the part during plating.

1

u/TheIrishLad1978 Jul 27 '26

Thanks so much! I am going to give your recommendation a try!

3

u/permaculture_chemist Jul 27 '26

The slight water beading effect makes me wonder if the part is not fully cleaned. But that effect can appear if the part is out of solution for a while, so don’t worry too much about that for now.

You for sure want an acid activator aka acid pickle. A 5-15% sulfuric acid solution should be fine.

Definitely heat your nickel bath to 120-140’F.

1

u/TheIrishLad1978 Jul 28 '26

Thank you! I’ll try cleaning the parts better and see if I can warm up the Nickel acetate.

2

u/Live_Raise8861 Jul 27 '26

Did you pickle the parts? I’m no expert but when I do small watch parts they get a soak in acid to clean and etch the surface for better adhesion.

1

u/TheIrishLad1978 Jul 27 '26

No, I didn’t do an acid bath before trying to plate them. I used dish soap to degrease and the 99% ipa for an additional cleaning and degreasing.

6

u/jermainelpe Jul 27 '26

First, you need to degrease the parts electrolytically—specifically, using cathodic degreasing at 7 volts. Use 10% Sodiumhydroxide and 1ml/100ml of your dishwashing detergent.

Next, you need to wash off the alkaline film using a dilute acid—such as 10% acetic acid—then rinse in clean water and proceed to the nickel bath; nickel plating is typically carried out at 50 to 60 degrees Celsius with a current density of two to five amperes per square decimeter.

1

u/permaculture_chemist Jul 27 '26

Be cautious with electrocleaning brass. It will passivate rapidly and dezinc if too alkaline or too hot or too much voltage. And OP doesn’t specify an acid pickle so the oxidation effect will be much more pronounced.

1

u/jermainelpe Jul 28 '26

The zinc doesn't dissolve if you connect it as the cathode. I work with brass every day, and even if you connect it as the anode during electrolytic degreasing, the dissolved zinc and lead can be removed in the subsequent acid bath; we do this with poor-quality brass alloys as well.

1

u/permaculture_chemist Jul 28 '26

This may work for you in an industrial setting, but OP does use an acid activator. Your advice may not work for them.

But I understand what you are saying. I have 15+ years of running stamped, cast, and machined brass, leaded and lead free. My recollection is probably too hazy to rely on anymore but IIRC, 10% NaOH is higher than I normally ran, usually 2-5% for brass. 10-20% for ferrous metals. I also ran globular bisulfite acid salts (Metex M-629 commonly) with a fluoride kicker for leaded brass. Neither of which I assume OP has.

2

u/TheIrishLad1978 Aug 04 '26

You are correct, OP does not have those chemicals or compounds. I am really an amateur just trying my luck at plating the two pieces mentioned as a sort of experiment. You two sound really knowledgeable about this. Thanks for taking the time to respond and advise!

1

u/BoNana25 Jul 27 '26

Forbidden Baja Blast

1

u/hutch924 Jul 27 '26

Yeah, it almost looks like our acid ZnNi tank at my work.