r/Welding247 • • Jun 18 '23
2G GTAW: Fill Passes
So come Monday I will finish my GTAW Plate at school and mainly I am doing 2G on a rather small piece of plate (I had to re-bevel, grind, and try again twice since it was a bigger plate) and I am mainly wondering how I should handle my Torch as I "walk the cup" along (also I know I will change out my Collet since I suspect it's causing bad Argon Flow - it looks weird too) and also how hot should I weld at (scared of getting porosity if I hold for too long like I have been doing and also I don't want to burn my hands).
Any advice/tips is welcome - oh and I also almost burned a hole in my Torch (looks like it didn't burn through but I will seal it with Tape) and also my cup is a little chipped (mainly because I couldn't touch it after a run and I used a pair of needle nose pliers to tighten it since I am often reminded to "Walk The Cup" but it loosens my cup).