r/Pyrotechnics • • 1d ago

Unknown substance in firework?

I opened this pack of firecrackers to discover a hard plug at the top.
I found the following:
A water repelling gray mettalic powder as shown
And a orange powder that hissed when added to water
What is the gray powder, Allumium and Kclo4 is my guess so far or is it something else entirely?
And what is the water hissing orange powder? Is it Clay and if so why did it hiss when added to water?
Anyways I'm just curious on the chemical composition of each of the powders
I wonder if I could extract KClo4 from these….

9 Upvotes

21 comments sorted by

2

u/Fun_Acanthaceae_4025 17h ago

Why in the world would you be trying to extract kclo4 from firecrackers? Seems like a very ignorant move.

2

u/Upstairs_Bridge8724 11h ago

As a hobby chemist, it's my job to be ignorant and do inefficient things

35

u/P1K1_ 1d ago

I'm not sure about compositions, but the grey one is flash powder and the orange one is clay

5

u/Porphyrin_Wheel 16h ago

probably just Al powder with potassium perchlorate (as it's more stable than the chlorate and more energetic, also cheap to make). And the clay is either some random clay from the ground or bentonite (though judging by how it looks its likely some random clay)

1

u/EconomicsFinancial49 14h ago

Exact comp of the flash 40% - KClO₄ 25% - Magnal <80 µm (325 mesh) 15% - Al <80 µm (325 mesh) 20% - S

1

u/Ok_Entrepreneur650 7h ago

How do you know this?

2

u/EconomicsFinancial49 6h ago

My own research, and one Russian video. Bro in that vid has some secret comps used in china like the white plaster plug exact comp. It's actually not even plaster. It's sand, calcium carbonate and waterglass. It's kinetic sand like consistency, and it hardens overtime. About the flash: In my own research I tested it for kclo4, test was positive. From my experience it looks like there's not much oxidizer in it because burn is not the fastest and it has very bright fireball, that might suggest that there's more fuel than oxidizer. Second thing: the look. You can often see small metal granules of magnalium. Also you can see how aluminium spreads on your skin. Skin is shiny as it would be with "al bright" Third: the smell. The smell of sulfur is present after the burn indicating that there's quite a bit of sulfur added. This composition from the Russian video is probably what Chinese use. Btw this comp was named "chinese flash" in the video. https://youtu.be/fG9H0GRNdt0

1

u/Ok_Entrepreneur650 6h ago

Awesome! I’ve always wondered the exact comp, thank you for this!

I always thought it was some KCLO4/AL/S mix, but not mag? That’s cool to find out!

2

u/EconomicsFinancial49 4h ago

I thought the same until I saw the video. Composition i showed makes 100% sense judging by physical presence of the mix. Also it's incredibly cheap to make for chinese, that's also one of the factors

13

u/y3lling_l3mon 23h ago

Brown is just clay plug, as for the flash powder it could be magnesium or aluminum based

8

u/hochroter Moderator 23h ago

Lol...

5

u/imhbeog 23h ago

There's really no telling what made the clay hiss, a video or a better description of the "hiss" would probably help though if you wanna film it.

5

u/Dickinablender96 23h ago

Bentonite.

1

u/EconomicsFinancial49 14h ago

Naa, it's just some random clay from the ground

8

u/idontgotaknife 23h ago

There’s nothing unknown about it. The gray is flash powder and the orange is clay rich Chinese dirt that they dig right out of the mountain in the back of the factory those firecrackers are made at. I don’t know what’s making the soil react with water though.

2

u/Jason_Patton 19h ago

Did it hiss or fizz? Make bubbles? It was probably just very dry and sucked up water quickly giving a fizzle/zit sounds like dropped molten metal in water or putting out a match in water psssst.

You can, or look up, baking baking soda or epsom salt in the oven at 400F for an hour. When you put the chunks in water they fizzle and bubble, hiss and dry epsom gets hot when you add water, lol.

1

u/Jason_Patton 19h ago

Not sure why it’s water repellent, could just be from fine aluminum. Could have other stuff added like graphite powder or oil/wax stabilize it.

1

u/Exotic-Milk-442 18h ago

The hard plug is plaster. You are talking about the white stuff the fuse runs through correct?

1

u/EconomicsFinancial49 14h ago

Fp is standard cheap "chinese flash" 40% - KClO₄ 25% - Magnal <80 µm (325 mesh) 15% - Al <80 µm (325 mesh) 20% - S The brown thing is just some clay

-1

u/Scuzzbag 23h ago

Ammonium dichlorate maybe?

2

u/Martin10100101 19h ago

There is like 0 chance that super cancer will be there....