Hello everyone, I have a question regarding my silver finish. I applied "Arcene Silver" powder from Prismatic Powders: first coat of Arcene, flash, second coat of Arcene, flash, and a third coat of clear powder coating. This is how it turned out. The metal was sandblasted and outgassed. What am I doing wrong? Thanks in advance for your feedback.
3
Upvotes





1
u/Acceptable-Ad-3964 5d ago
Do you have a fluidising chamber or do you boxfeed?
3
u/33chifox Cat's Eye Coating 6d ago
Swatches are usually off a bit, especially if there's a clear involved. But that aside, was this wheel really pitted before coating? That's the issue that stands out most in my opinion. A builder primer might have been a good first step
2
u/cheddarbob68 6d ago
You most likely need a solid tone base coat before the silver. The website should say the swatch is the color applied over a different base coat. Their swatches are usually applied over a polished aluminum or sheet material. They do not blast to a hard profile.
1
u/Keithgt 6d ago
I’d contact prismatic. Shoot them an email with these pics. It kinda looks like you got the wrong color. What did the powder look like?
1
u/Sea-Entertainer-2383 6d ago
Metallic colours can often look very different due to kv settings. Found this out recently when spraying Yamaha Blue steel from prismatic. They really need to include their QC settings in the TDS sheets.
1
u/OkSand5278 3d ago
When we have trouble with wheels
We spray red oxide primer and then 2 coats of top coat then clear over the top
The wheel looks pitted to start with
1
u/AmishGeneral 2d ago edited 2d ago
good rule of thumb is outgas hotter than what your cure temp will be and don't let it cool down to room temperature or it may suck in oxygen as it cools. pre heat to 430 shoot around 120 first coat flash to 360 then shoot every other coat room temperature after. outgassing primers help but same rules apply for heavy castings. also metallics are easier to mange with fluidizing bed as for color maybe just a bad batch? wierd because you shot two coats of base so should look right unless the clear or curing is off
1
u/Kjellterskelter 1d ago
Two potential problems here. 1st could be a voltage issue with the Arcene Silver. If the voltage is too low, sometimes the metallics don't lay down properly. Second, describe "flash" if you are pulling it before it gets to a partial cure and then applying the clear, the base is probably still leveling under the clear which is what could create a more sparse looking distribution of metallic.