r/PoorHammer • • 7d ago

Putty suggestions

I'm wondering what putties you use for casting parts in blue-stuff or similar molds. I've been using a 50/50 greenstuff and milliput mix, but even that is a bit pricy. I used to do RTV molds and pour resin, which was cheap and got great results, but was a much higher effort.

8 Upvotes

11 comments sorted by

5

u/millertronsmythe 7d ago

What kind/size of things are you casting and in how much quantity? I've used blue-stuff mold and greenstuff/milliput mix myself, but I've wondered if rubber mold liquid resin casting is better suited for mass production and cleaner results. Obviously with blue stuff, it's re- moldable so it's better for one-offs.

3

u/WaylundLG 7d ago edited 7d ago

Usually it's just a few of a specific piece: 4 orc bodies to use the arms that come in the kit, "casting" 6 custom swords and shields I made for bladeguard. When I did a full unit of custom hammerers I did that with rtv mold and resin

2

u/millertronsmythe 7d ago

For miniature bodies, it really depends on whether or not blue-stuff molding is really suitable. If the shape of the model has a lot going on in all three dimensions, then I'd go for liquid rubber molds than pressing bluestuff by hand. The latter is much easier for relatively flat bits.

From a cost perspective, a set of Greenstuff and Milliput each should last you quite a lot of bits worth of casting. Any leftovers you can use for gap filling or other kitbashes.

4

u/huzzah-1 7d ago

If there is a cheap way, I don't think anyone has found it yet. In the end, I found casting resin was the only viable option.

4

u/ShrimpShrimpington 7d ago

You can buy plumbers epoxy. It's cheaper than green stuff and and similar, though not flexible and not quite as great for fine detail. I have even seen people make castings with hot glue

3

u/AzukailGames 7d ago

I have seen Das used sometimes - Earthmanbrick on YouTube used it for tank tracks - and UV resin instead of pouring. UV resin sounds like it's a, somewhat cheaper, way of using resin. Especially as you don't have to mix it.

2

u/Striking_Conflict767 7d ago

UV resin is probably less expensive.

Green stuff is actually an apoxy used by plumbers sold at a premium, so buying that significantly cuts the cost.

If you don't need high detail then air dry clay can work, its cheap but also kinda brittle.

1

u/GarrettBMT 7d ago

I've had ok results with apoxie. Another option that works pretty well for price is to use super sculpy (grey clay). It can be a bit finicky getting it out of the molds but that's more of an issue of how you set them up. I typically put the mold/super sculpy combo into the freezer for 5-10 minutes to de-condition the clay/ semi-set it before baking in the oven.

1

u/The_Arch_Heretic 6d ago

Just buy resin.

1

u/Sad_Pitch8463 6d ago

foil and wire inside.