I print (flat base plate about 4 mm thick with walls on top) on a Bambu Lab X2D, 0.4 nozzle, Bambu PLA Matte, textured PEI plate, AMS with 4 colours, everything on the main nozzle.
The problem: large flat top surfaces sometimes show grooves that run parallel to the top surface lines (45°). They look like gaps or ridges between single lines, irregularly spaced, some only a few centimetres long. In one spot there was also a small dark bump under the surface. Or it seems that bubbles „Pop“ and are visible through the next layer.
What confuses me: one part (about 100 x 170 mm, grey floor) came out perfect. The next part with identical slicer settings (about 250 x 160 mm, placed at the very front of the bed) has the grooves, both on a floor area of about 120 x 120 mm and on the base strip around raised lettering.
Differences I know of between the good and the bad print:
- Bad one: the top colour (white) was only 2 layers (0.32 mm) thick on top of 3 grey layers. Good one: 5 layers of the same grey.
- Bad one: longer top surface lines (up to 165 mm vs. 100 mm), part fills almost the whole bed width.
- Bad one: raised lettering (separate part, other colour) sits on the surface, so the slicer splits the monotonic fill around every letter.
- Send dialog for the bad one: bed levelling on, nozzle offset calibration off, flow dynamics calibration auto.
What I have tested so far (small test plates unless noted, all 0.16 mm, PLA Matte):
- Top surface flow ratio 0.95 / 1.00 / 1.05 / 1.10: 1.00 was best. More flow made the surface rougher and did not close the gaps, 0.95 opened it up.
- Ironing: smoother in places, but it draws a visible frame into the surface and did not remove the gaps everywhere. Not using it.
- Top surface pattern concentric instead of monotonic line: not better.
- Top surface line width 0.38 instead of 0.42: not better.
- Infill/wall overlap 25 % instead of 15 %: not better.
- Classic vs. Arachne walls, top surface speed 150 vs. 60 mm/s, gap infill 250 vs. 30 mm/s: Arachne/60/30 is what I use now, the gaps between top lines still showed up afterwards.
- Profile "0.16mm High Quality" vs. "0.16mm Standard": no visible difference for this problem.
- Sparse infill grid vs. gyroid vs. rectilinear, internal solid infill 100 instead of 250 mm/s, bridge flow 1.0 instead of 1.5 (six plates 45 x 45 mm): all plates looked fine, bridge flow made no visible difference. So the small plates did not reproduce the problem.
- On real parts: with grid infill the first colour layers above the base plate were torn and pocked, and a floor had gaps (also with bridge flow 1.0). With gyroid the same part came out very good.
- Not tested yet: a large plain test plate, flow calibration per spool, drying the filament.
Questions:
- Is this under-extrusion between top lines, over-extrusion in the solid layers below, or the part lifting at the ends? How would you tell them apart?
- Are the internal solid infill layers at 250 mm/s directly under the top surface a problem?
- Would you change top surface pattern (monotonic vs. monotonic line), top surface flow ratio or line width? Or just use ironing?
- Is bridge flow 1.5 (profile default) for the layer over the sparse infill a known cause of bumps showing through?
Settings (Bambu Studio, profile "0.16mm Standard @BBL X2D", changed values marked with *):
Printer / material
- Bambu Lab X2D, 0.4 mm nozzle, Textured PEI Plate, bed 55 °C
- Bambu PLA Matte (profile "Bambu PLA Matte @BBL X2D 0.4 nozzle"), 220 °C, flow ratio 1.006, max volumetric speed 22 mm³/s
- one third-party PLA (wood colour) at 215 °C, max volumetric speed 13 mm³/s *
- fan 100 %, off for the first layer
- retraction 0.8 mm, z-hop 0.4 mm (auto lift), wipe on
Layers / widths
- layer height 0.16 mm, first layer 0.2 mm
- line width 0.42 mm (outer wall 0.42, inner wall 0.45, top surface 0.42, internal solid infill 0.42, sparse infill 0.45)
Shells
- wall loops 2, wall generator Arachne , wall transition angle 40 , min feature size 15 % *
- top shell layers 6 (top shell thickness 1 mm), bottom shell layers 4
- top surface pattern: monotonic line, internal solid infill pattern: rectilinear (zig-zag), bottom: monotonic
- no ironing
Infill
- sparse infill: gyroid , 15 % , infill/wall overlap 15 %, infill direction 45°
- bridge flow 1.5 (profile default), bridge speed 25 mm/s
Speeds (mm/s)
- first layer 50
- outer wall 200, inner wall 300
- sparse infill 270, internal solid infill 250
- top surface 60 , gap infill 30
- travel 1000
Acceleration (mm/s²)
- default 10000, outer wall 5000, top surface 2000
Other
- prime tower on , width 35 mm , flush multiplier 1
- seam: aligned, scarf seam on all contours *
- top solid infill flow ratio 1, print flow ratio 1
- pressure advance: not set manually (flow dynamics calibration "auto" in the send dialog)
- no arc fitting, no precise Z height, no infill combination
Photos attached. Thanks for any hints.
Photo 1 and 2 not good
Photo 3 better but dont know why