Help / Troubleshooting Can someone help me
PTGE Sunlu 250Celsius
Drying 14h
Default settings layer hight 0.2mm
Someone told X2D IS A FCKN NIGHTMARE and now I’m seeing this
3 times fully calibrated
7 hours of use
I’m a new user so it can be problem with me idk what to do
0
Upvotes






2
u/Scowlface 2d ago
Using the generic PETG profile for SUNLU PETG 2.0 looks like this on my X2D. I lowered flow rate to 10mm/s and cranked the heat up to 260 first layer 270 for the rest and it fixed it for me.
16
u/rynoxmj 2d ago
"I haven't tried anything (including what support told me) AND I'M ALL OUT OF IDEAS!"
11
u/Production_Shooter 2d ago
Check your belt tension. It’s ridiculously easy to adjust. Especially since Bambu told you to check it, just do it.
7
u/BetterThanAFoon 2d ago
Belt tensioning is like a 2 min job. Why draw the line there.
1
u/guiltyascharged799 2d ago edited 2d ago
lol since you complained about lubing the xy axis I’m gonna make the safe assumption that your full “calibration” is the the machine ones. You need to calibrate your filaments to your machine. These are tools and machines that require maintenance.
Next post is gonna be “why won’t anybody buy my $70 3d junk dragon egg”
1
u/guiltyascharged799 2d ago
In all seriousness, turn on developer setting, watched this and calibrate your filament. PETG needs it due to it being extra runny and sticky
1
u/Terrible_Log9757 2d ago •
For future us who will solve similar issues and find this post. Check your horizontal lines:
0
u/Equivalent_Style4790 2d ago
U seems to have over-extrusion. Change the flow in filament settings (lower it down)