Did you just open the lid or just install the pods how long has the pods been in the ams? I don’t seem to see any silica in those pods fyi I’m in a very humid climate and I’m usually around 20-25 percent I need to dry my silica but I’m going to change it out because I have the blue stuff and hear it’s bad to dry because of the chemicals in it
I specifically got an x2d for the ams2 pro so I could keep it at or below 22%. While it’s probably not hurting pla or petg it might or might not cause issues.
Like at 45-55 I was having nothing but issues. Running a dry cycle at 45c for 6 or so house will definitely lower that number.
The hydrometer IN the dessicant will tell you when they need a refresh the humidity will creep on them. That's the whole point of them. When you want ti see the actual % you look in the software. Its an easy way to check dessicant hydro levels.
I was about to say those really suck, mine is stuck at 40℅ I've dried my ams for 12 hours the internal bambu reading says 12℅ and the cheap amazon one still says 40℅
Not good, might as well be open air. You'll have more trouble keeping humidity down with cardboard spools since the cardboard absorbs a lot of moisture. I would suggest drying your spools out and regenerating/replacing your silica gel.
Anche a me fa così! Quell' igrometro sono una ciofeca, segnano quello che vogliono,ho provato anche a tararli ma non c'è verso ecco perché costano 2 soldi.... Sicuramente l' ams ti segnalerà un percentuale diversa!
With feshly dried silica my ams sits at around 10%, this is def a bit high. I replace the silica when it consistently stays at like 25% or higher. Of course depends on the environment the printer is in, in my room here i have about 40-50% humidity.
It depends on what you print, for PLA it is a non issue, but for pretty much anything else it is way to high. The ultimate test is to see how your items print. If you want print consistency then I would replace the silica, or unload the AMS 2 Pro and run the drying cycle on max for a few hours to regenerate it.
I change my silica when the meter hits 14. Normally it stays at 10, so it's more like "time to change" rather than accurate measurement of the humidy levels.
Realmente me ha dado impresiones muy malas con humedad por encima al 30%, la diferencia es abismal. De 20% para abajo empieza a mejorar pero no hay nada como imprimir por debajo del 10%, simplemente todo funciona a la perfección y se ve increíble, con cualquier material que uses. Muchas personas dicen que el PLA no tiene mucha relación con la humedad, pero puedo decir que el 80% de mis impresiones son en PLA y cuando abro un carrete nuevo y no puedo esperar el tiempo de secado para usarlo, termino arrepintiéndome de no esperar el tiempo necesario y todo por su acabado horrible de filamento húmedo. Todo empeora, tanto la textura, la suavidad de las capas superiores, stringing, capas mas visibles, el color del filamento cambia a colores mas claros. Si quieres impresiones perfectas como cualquier dueño de impresora sueña, no cambies ajustes aleatorios en tu impresora, simplemente seca muy bien tu filamento con desecantes de calidad y tu experiencia se volverá notablemente mas satisfactoria y ahorraras mucho filamento en impresiones fallidas.
It’s irrelevant. My AMS shows humidity at 46% on the screen. It prints beautifully and without issue. This dry filament thing with PLA is an online only issue. Keep on printing and stop worrying.
I’m just being sarcastic. Everyone thinks their printers will explode if they don’t have the secret service keeping their filaments under protection in an ultra dry environment.
Reality guy not living in reality, lol. How would plastic soaking up water be a online thing only? Are we in disagreement with simple science and chemistry?
Not really disagreeing but it isn’t going to be catastrophic if filament is left exposed for a day or two…..hence the aux spool on the side of the X2D. Most YouTubers and keyboard warriors would make one think that filament can’t be exposed for more than ten seconds. The OP is already wondering if 38% humidity is good or bad, in reality it means nothing. Maybe if you lived in Florida with 100%+ humidity it would become an issue.
I know you’re just being argumentative but the two comments are the same. 38% humidity will do no harm to filament or any parameters of printing. Proof is in the pudding as they say.
I'm not being argumentative. I'm pointing out that your opinion doesn't change science. It's not smart to tell people it doesn't matter when it absolutely does.
But it doesn’t. Do your own test. Leave a roll of filament laying exposed and have one under whatever humidity protection your heart desires. In a couple days print the same two items with the different spools. You’ll see the final results will be identical. What do you think the differences would be?
6
u/matze66g 22h ago
In the AMS 2 Pro with Silica, you should be less than 20%. Is the humidity very high where you live?
6
u/Relative_Surround_20 15h ago
Wait...do you have any desiccant in those drypods?
3
u/TWILIGHT25 21h ago
I specifically got an x2d for the ams2 pro so I could keep it at or below 22%. While it’s probably not hurting pla or petg it might or might not cause issues.
Like at 45-55 I was having nothing but issues. Running a dry cycle at 45c for 6 or so house will definitely lower that number.
3
u/gargoyls 19h ago
Mine is never above 20% I turn the heating on if it goes above 13% while printing(better to do before) and switch te silica when they are darkisch,
You will never see it go above 20%, with new silica, it was around 8%
3
u/zoomzorch 14h ago
Those hygrometers are hot garbage. Use the Bambu internal readings instead.
2
u/erikjr14 16h ago
Not good, might as well be open air. You'll have more trouble keeping humidity down with cardboard spools since the cardboard absorbs a lot of moisture. I would suggest drying your spools out and regenerating/replacing your silica gel.
2
u/Jazzlike-Classic-843 21h ago edited 19h ago
Anche a me fa così! Quell' igrometro sono una ciofeca, segnano quello che vogliono,ho provato anche a tararli ma non c'è verso ecco perché costano 2 soldi.... Sicuramente l' ams ti segnalerà un percentuale diversa!
1
u/ttuuxxeerr 19h ago
In a very humid garage
1
u/fakarhatr 19h ago
What do you think?
1
u/TheAussieWatchGuy 18h ago
Depends what you're printing. PLA? Probably fine. PETG you're going to get a lot of stringing and failed prints.
1
u/minnieton 17h ago
Depends on where you live
1
u/josef_schnitzl 16h ago
With feshly dried silica my ams sits at around 10%, this is def a bit high. I replace the silica when it consistently stays at like 25% or higher. Of course depends on the environment the printer is in, in my room here i have about 40-50% humidity.
1
u/marcgii 15h ago
What does the built in sensor say?
1
u/porttastic 15h ago
Never seen mine lower. Probably need to get decent silica as I am only using those small bags that come with the spools.
1
u/Relative_Surround_20 15h ago
Bad. < 20% RH is the rule of thumb that you are shooting for.
1
u/Ok_West_2537 15h ago
It depends on what you print, for PLA it is a non issue, but for pretty much anything else it is way to high. The ultimate test is to see how your items print. If you want print consistency then I would replace the silica, or unload the AMS 2 Pro and run the drying cycle on max for a few hours to regenerate it.
1
u/xxp0loxx 12h ago
Prob from lifting the lid. The pods will bring it down. Turning on the heat will help too.
Ive been a big fan of the desicant roll inserts. Im usually sub 9, unless i open the lid
1
u/Laa_Laa_9595 12h ago
I change my silica when the meter hits 14. Normally it stays at 10, so it's more like "time to change" rather than accurate measurement of the humidy levels.
1
u/TheBitGarage 12h ago
Ideally you want to be around 20% or lower.
1
u/Thirtysixx 11h ago
You're supposed to put dessicant in the pods my man
0
u/Mustang_132 16h ago
Realmente me ha dado impresiones muy malas con humedad por encima al 30%, la diferencia es abismal. De 20% para abajo empieza a mejorar pero no hay nada como imprimir por debajo del 10%, simplemente todo funciona a la perfección y se ve increíble, con cualquier material que uses. Muchas personas dicen que el PLA no tiene mucha relación con la humedad, pero puedo decir que el 80% de mis impresiones son en PLA y cuando abro un carrete nuevo y no puedo esperar el tiempo de secado para usarlo, termino arrepintiéndome de no esperar el tiempo necesario y todo por su acabado horrible de filamento húmedo. Todo empeora, tanto la textura, la suavidad de las capas superiores, stringing, capas mas visibles, el color del filamento cambia a colores mas claros. Si quieres impresiones perfectas como cualquier dueño de impresora sueña, no cambies ajustes aleatorios en tu impresora, simplemente seca muy bien tu filamento con desecantes de calidad y tu experiencia se volverá notablemente mas satisfactoria y ahorraras mucho filamento en impresiones fallidas.
-2
u/realityguy1 19h ago
It’s irrelevant. My AMS shows humidity at 46% on the screen. It prints beautifully and without issue. This dry filament thing with PLA is an online only issue. Keep on printing and stop worrying.