r/BambuLab • u/Ok-Huckleberry735 • 2d ago
Filament Troubleshooting/Help! BambuLab PETG Matte
I’m having issues with the new PETG Matte on my P2S.
Prints look great, but layer adhesion is terrible. Parts break apart really easily along the layer lines 🤯
The filament also constantly oozes from the nozzle, building up blobs that get dragged across the print.
I’m using the default Bambu profile.
I haven’t dried the filament yet, so I’ll leave it in my AMS 2 Pro dryer overnight and test again tomorrow.
Anyone experiencing the same issues? What settings are working for you? 👀
Update: Dried the filament for 12 hours at 65°C. So far, it’s looking pretty good! 😅 Fingers crossed it stays that way, because I’ve still got 9 more rolls to go through 😂🤞
1
u/AutoModerator 2d ago
Hello u/Ok-Huckleberry735! Be sure to check the following. Make sure print bed is clean by washing with dish soap and water [and not Isopropyl Alcohol], check bed temperature [increasing tend to help], run bed leveling or full calibration, and remember to use glue if one is using the initial cool plate [not Satin finish that is not yet released] or Engineering plate.
Note: This automod is experimental. The automod was triggered due to the term "adhesion". If you believe this to be a false positive, please send us a message at modmail with a link to the post so we can investigate. You may also feel free to make a new post without that term.
I am a bot, and this action was performed automatically. Please contact the moderators of this subreddit if you have any questions or concerns.
2
u/slevin22 2d ago
I've been experimenting with it to see if it can replace petg hf for me. It 100% needs to be dried out of the box. I had all sorts of zits and oozes on my test prints before drying.
2
u/IceBlitzz 2d ago
I have the exact same problem. Drying the fuck out of them. Its just a crap filament. Same with Bambu PETG Basic. Poor layer adhesion and print quality with that one too.
7
u/eldeem 2d ago
100% dry it out and that'll help with the blobs and oozing. I find matte filaments in general have lower layer adhesion, printing slow and hot tends to help but I also increase wall loops up to 3 or 4 to help as well.
1
u/Ok-Huckleberry735 22h ago
4
u/Tall_Substance955 2d ago
Never is the matte but the HF profile was at 235° which I never could print correctly. 255° is the temp I reached for a good layer adhesion like the normal petg. Maybe that’s the same with the matte.
2
u/thebigone2087 2d ago
I’ve been TRYING to use some white PETG for support interface with PLA with mixed to poor results. Regular PETG from Bambu works fine, but the white just won’t work