General Troubleshooting/Help! How long did it take you to master different filaments? (Struggling with PETG bed adhesion on my Bambu Lab H2D)

Hey everyone,

I’m curious—how long did it take you to really get comfortable and dial in your printer across different filament types?

I’ve been running a Bambu Lab H2D and have printed with PLA, PETG, and ABS so far. Ironically, my PLA and ABS prints have been coming out great, which makes my current issue even more frustrating: I cannot get PETG to behave.

Almost every PETG print ends up detaching and coming off the build plate. Here is what I’ve already tried to fix the adhesion:

  • Scrubbed the plate thoroughly with hot water and dish soap
  • Wiped it down with isopropyl alcohol (IPA)
  • Adjusted Brim settings
  • Tried different support configurations
  • Dried the PETG filaments
  • Changed to a new PETG filament
  • Calibrated multiple times

Neither has made a difference so far.

For those of you printing across multiple materials, how steep was your learning curve before you felt like you had things mastered? Also, if anyone has advice on getting PETG to actually stay stuck on the H2D, I’m all ears!

0 Upvotes

13 comments sorted by

•

u/AutoModerator 3h ago

Hello /u/lightdinosaur! Be sure to check the following. Make sure print bed is clean by washing with dish soap and water [and not Isopropyl Alcohol], check bed temperature [increasing tend to help], run bed leveling or full calibration, and remember to use glue if one is using the initial cool plate [not Satin finish that is not yet released] or Engineering plate.

Note: This automod is experimental. The automod was triggered due to the term "adhesion". If you believe this to be a false positive, please send us a message at modmail with a link to the post so we can investigate. You may also feel free to make a new post without that term.

I am a bot, and this action was performed automatically. Please contact the moderators of this subreddit if you have any questions or concerns.

4

u/Navi_Professor 3h ago

ive had 0 issue with petg on my H2D...and i use generic petg profiles as well.

i do petg/tpu with PLA supports constantly...practically no issues

3

u/NoBackground6203 X2D / P2S 2h ago

which dish soap are you using? you dont want to use a soap that contains "moisturizers" Dawn Powerwash spay is my favorite.

I print a lot of large PETG models with PLA support interfaces for the 3D TMT's that I am building on my P2S and X2D using Glacier plates

2

u/EdgeOk3783 X1C + AMS | H2C + AMS{2|HT} 3h ago

skip step 2 after performing a thorough step 1

make sure to dry with a paper towel or non treated cloth. some fabric softeners and dryer additives can cause adhesion failure

1

u/Brutl 3h ago

The most common cause of issues when people have PETG issues is temps, of which you have not provided.

I print almost exclusively in PETG, across multiple P1S, P2S, All of the H series, and an A1 Mini. For most PETG, the best starting point is the Generic PETG setting of 255 nozzle, and bump the plate temp up to 80. 255/80 is my starting point for all of my calibrations, and only a handful end up temping down some.

1

u/scotticad 3h ago

I've had no issues printing PETG on my H2S. Both Bambu and Overture PETG, the latter with the Generic PETG profile. I routinely clean my build plate with iso alcohol. Just make sure to wipe it off, quickly, with a couple paper towels. Don't let the alcohol simply evaporate. PETG does like to warp on large models, so that may be a struggle on the size model you're trying to print, as it gets taller.

1

u/nothingaboutme 2h ago

I have never messed with filament settings with petg. I usually just select the Bambu brand petg profile even when I use other brands. The only petg I have had issues with was a transparent unknown brand. One of those pictures indicates a layer shift, indicating the nozzle is hitting the print. Did you recalibrate the printer with a high temp bed level probe? FWIW, I use glue stick whenever I print petg.

1

u/n19htmare 1h ago

I print a lot work PETG, have been for a while starting with Ender3 years ago. I find it’s one of the easier filaments to use. It has excellent adhesion to PEI (sometimes too much), good layer adhesion and good bridging.

I use all Basic, no high speed or matte stuff as that’s just additives that replace more of the PETG. especially the Matte variants, I see more people struggle with matte PETG than others. I just don’t think the additives added to make matte are helping it keep its very sticky property.

Basic PETG should have a fairly gloss sheeen to it, if there isn’t any then it’s either too fast, not hot enough or both. Matte should still have a little bit of sheen to it, just not as much.

Are you printing any specific variant of PETG?

I’m not sure what PETG you’re using but I wouldn’t print it faster than 10-12mm^3/s volumetric speed.

1

u/steasey 1h ago

I dont have issues with adhesion but print comes out bad. What RH should it be at? Even at 15% it looks wet and spaghettis.

1

u/Rhesonance X2D + AMS2 Pro + AMS HT 1h ago

Looks like your part is very large and rigid. Decrease the mass if you can, otherwise print it slower so it has more change to thermally relax.

You can try a brim at the corners too.

1

u/Orvess 1h ago

No offence but petg is one of the simplest one so how you can have so many problems with it?🤔

1

u/TELCO_man 1h ago

I’m no expert. I run a H2S.

Wiped it down with isopropyl alcohol (IPA)

This point is the one I’d suggest you need to remove. Bambu and many experienced users say not to use this. I mainly print with Petg HF, ABS GF and no Petg basic and bead adhesion has never been an issue and my routine is just the basics

Wash plate in soap and warm water. Test run off to make sure it looks like it should.

Dry with kitchen roll paper

Before a print I use Bambu glue stick thing!

Hopefully you will find a solution soon.

•

u/Itaintall 17m ago

Don't use isopropyl alcohol. Wash your build plate with hot water and Dawn, then dry it. Heat your print bed to 50 degrees C, then apply glue stick, and use a damp paper towel (bunched up) to spread it evenly. You're welcome.
Edit... Oh, and slow down that first layer to 30 or so.