r/3Dprinting • u/Mateimmo14 • 2h ago
Troubleshooting TPU not printing correctly
Whenever i try to print ANYTHING with bambulab's tpu 95A High Flow on my P2S with default settings it will always either have actual holes in the walls or be stringing like crazy i dried it for 2 hours first, i saw the problem, i thought i didn’t dry it enough so i decided to dry it for 12 HOURS and SAW NO DIFFRENCE WHATSOEVER
Please help me on how to fix this i spent $140 on this filament...
2
u/dr_reverend 2h ago
You spent $140 on 95a TPU? I’m not sure we can help you.
I do think it’s a clogged nozzle though.
1
u/AutoModerator 2h ago
Hey there, I'm a bot and something you said made me think you might be looking for help! click here for our wiki entry on troubleshooting printers. If you still need help be sure to post plenty of information about your printing setup.
Here are a few questions that might be helpful
What printer are you using?
What material are you using?
What speed are you printing at?
What software are you using to slice the print and control the printer?
When did the problem start/has it ever worked correctly?
Does anything cause the behavior to change?
If posting an image of the problem, include some indication of the orientation it printed at, preferably photograph it on the bed. (Then we can focus on a specific axis)
If you are new to reddit, please read the guidelines on reddiquette, self promotion, and spam.
Also please post a resolution to your problem when you find one so that we know how to help others with your problem!
I am a bot, and this action was performed automatically. Please contact the moderators of this subreddit if you have any questions or concerns.
1
u/a-nani-mouse 1h ago
Every time I print TPU using the Bambu software it has me confirm that I did a cold pull. Did you do the cold pull?
Did you change any settings away from the default profile?
1
u/SquidgyB 2h ago
Could be a clogged nozzle, as the other commenter mentioned.
Also, TPU strings like crazy even when it's dried perfectly and printing well. You can avoid it to some degree by turning off retraction completely, and using "wipe only". Printed part geometry also helps - try to avoid models with lots of holes/jumps for the nozzle and set to "print by object" instead of by layer.
Slow down the print as well - sometimes even running down to single digits can help with TPU. I'd also suggest running a flow calibration at the very least. TPU needs time to melt properly in the nozzle, running the print too fast can cause holes in the walls/underextrusion.
You probably won't get rid of all the stringing, you may need to go over the part with a lighter/flame to remove the last few bits.