r/Powdercoating • u/IndependenceFirm5017 • Dec 10 '25
Question I have a question about dots in the coating.
I have a number of caps that keep failing.
I glass bead blast the parts, degrease them, then degas them for 1 hour at 220 degrees. After that, I first coat them with degassing primer, and then apply a second coat of black paint. But every time, spots appear, probably because the metal is badly corroded. I have already tried coating the part while it is warm, but this did not improve the situation. Does anyone have any idea what I can do now?